Holes or pillowing in the top surface

By Tony Tate · updated 2026-11-27 · First Layer 1.0.2

Most often it is one of these: not enough top layers, or infill density too low to support the top. Use at least 4–5 top layers. The full list below is ordered by how often each cause is actually to blame, so work down it rather than picking the interesting one.

The top solid layer has gaps, or bulges upward between infill lines.

gaps in top layerrough topyou can see the infill

Causes, most likely first

Ordered by how often each is actually responsible, not by how interesting it is. Work down the list.

Not enough top layers

Use at least 4–5 top layers. Solid layers need something to span onto.

Infill density too low to support the top

Raise infill to 15–20%. Top layers are bridging across the infill gaps.

Under-extrusion

Calibrate flow.

Calibration step: Calibrate flow ratio / extrusion multiplier →

Not enough cooling on the top surface

Raise the fan for solid top layers so each bridged line sets before the next.

Common questions

What causes holes or pillowing in the top surface in 3D printing?

Not enough top layers. Use at least 4–5 top layers. Solid layers need something to span onto.

What else causes holes or pillowing in the top surface?

Infill density too low to support the top. Raise infill to 15–20%. Top layers are bridging across the infill gaps.

How do I know if it is fixed?

Change one thing at a time and reprint the same test. The top solid layer has gaps, or bulges upward between infill lines. If that is gone, the change you made was the cause; if it is not, undo it before trying the next one.

Open First Layer →
The app walks this in order, generates the test model for your nozzle and filament, and records what you measure so nothing has to be repeated. Free, no account, works offline.