Most often it is this: flow multiplier too high. Run the flow cube and calculate it: new_flow = old_flow × (target / measured). The full list below is ordered by how often each cause is actually to blame, so work down it rather than picking the interesting one.
Bulging walls, a rough or ridged top surface, and outer dimensions measuring oversized.
blobbyrough top surfacedimensions too bignozzle plowing
Ordered by how often each is actually responsible, not by how interesting it is. Work down the list.
Run the flow cube and calculate it: new_flow = old_flow × (target / measured).
Calibration step: Calibrate flow ratio / extrusion multiplier →
Measure the real diameter at five points and average. Entering 1.75 when the filament is 1.70 over-extrudes by about 6%.
Recalibrate e-steps before touching flow — flow tuned on wrong e-steps is a compensating error.
Abrasive filament widens a brass nozzle over time. Replace it, and use hardened steel for anything filled.
Flow multiplier too high. Run the flow cube and calculate it: new_flow = old_flow × (target / measured).
Filament diameter wrong in the slicer. Measure the real diameter at five points and average. Entering 1.75 when the filament is 1.70 over-extrudes by about 6%.
Change one thing at a time and reprint the same test. Bulging walls, a rough or ridged top surface, and outer dimensions measuring oversized. If that is gone, the change you made was the cause; if it is not, undo it before trying the next one.