Most often it is one of these: nozzle temperature too low, or too much part cooling. Run a temperature tower and choose for LAYER ADHESION, not looks. The full list below is ordered by how often each cause is actually to blame, so work down it rather than picking the interesting one.
The part breaks cleanly between layers, or visible cracks open on tall walls mid-print.
delaminationcrackingparts snap along layer lines
Ordered by how often each is actually responsible, not by how interesting it is. Work down the list.
Run a temperature tower and choose for LAYER ADHESION, not looks. The prettiest band is frequently the weakest.
Reduce the fan. On ABS/ASA turn it off entirely — cooling is the direct cause of splitting on those materials.
A cold draught across a tall ABS part splits it every time. Enclose it.
Layers cannot fuse with insufficient material. Fix flow first, then re-assess.
Calibration step: Calibrate flow ratio / extrusion multiplier →
Steam bubbles at the nozzle interrupt the bead and weaken the bond. Dry the spool.
Nozzle temperature too low. Run a temperature tower and choose for LAYER ADHESION, not looks. The prettiest band is frequently the weakest.
Too much part cooling. Reduce the fan. On ABS/ASA turn it off entirely — cooling is the direct cause of splitting on those materials.
Change one thing at a time and reprint the same test. The part breaks cleanly between layers, or visible cracks open on tall walls mid-print. If that is gone, the change you made was the cause; if it is not, undo it before trying the next one.