By Tony Tate · updated 2026-11-27 · First Layer 1.0.2
Composite TPU (CF / GF filled) prints at about 235 °C with a 50 °C bed and 30% part cooling. Usable range 220–250 °C nozzle, 30–60 °C bed. No enclosure needed. Abrasive — needs a hardened nozzle.
starting points Every number here is drawn from
manufacturer data sheets across the material as a whole. None of it is a measurement of the
spool in your hand, and brand-to-brand variation inside one material is wider than most people
expect. Where a figure says "about", the app holds one typical value rather than a range. Treat
all of it as somewhere to begin, then measure — shrinkage and flow especially, because those two
are what throw dimensions off.
Nozzle
220–250 °C (start 235)
Bed
30–60 °C (start 50)
Part fan
0–50% (start 30%)
Wall speed
15–35 mm/s
Max volumetric flow
about 4 mm³/s
Shrinkage
about 0.5%
Glass transition
about -30 °C — flexible above it, so at room temperature it is rubbery rather than soft
Enclosure
Not needed
Nozzle size
0.4 mm or larger — 0.6 mm recommended
Nozzle material
Hardened steel required — this is abrasive
Drying
about 55 °C for 6 h
Speed
Slightly faster than unfilled TPU of the same hardness, 15–35 mm/s, because the fill stiffens the filament and it buckles less readily in the drive gear.
Bed surface
Clean smooth PEI at 50 °C.
Nozzle
HARDENED steel, and 0.6 mm. Chopped fibre in a flexible carrier is unusually hard on a nozzle, and a worn one shows up here as inconsistent extrusion long before it looks worn.
What bites people
Needs a hardened nozzle. Brass will not survive a spool, and the wear is invisible until every dimension has drifted.
Stiffer and tougher than unfilled TPU at the same shore rating — the fill trades elasticity for impact resistance and wear.
Feeds more easily than plain soft TPU for the same reason, which makes it a reasonable flexible to attempt on a Bowden machine.
Layer adhesion suffers where fibres bridge a layer line. Print hotter than you would the unfilled version.
Safety
Nozzle above 220 °C.
Abrasive fill — do not print through a brass nozzle.
Common questions
What temperature should I print Composite TPU (CF / GF filled) at?
Start at 235 °C nozzle and 50 °C bed, within a usable range of 220–250 °C and 30–60 °C. Run a temperature tower on your own spool rather than trusting any table: brand-to-brand variation inside one material is wider than most beginners expect.
Does Composite TPU (CF / GF filled) need an enclosure?
No. Composite TPU (CF / GF filled) prints fine on an open-frame machine.
What nozzle do I need for Composite TPU (CF / GF filled)?
0.4 mm or larger, with 0.6 mm recommended. It is abrasive, so it needs a hardened steel nozzle — it will wear a brass one wider as you print, which quietly invalidates every calibration you have done.