By Tony Tate · updated 2026-11-27 · First Layer 1.0.2
Wood-filled PLA prints at about 200 °C with a 55 °C bed and 100% part cooling. Usable range 185–220 °C nozzle, 50–65 °C bed. No enclosure needed. Mildly abrasive — brass copes, hardened lasts.
Wood PLATimberfillBamboo PLA
Starting settings
starting points Every number here is drawn from
manufacturer data sheets across the material as a whole. None of it is a measurement of the
spool in your hand, and brand-to-brand variation inside one material is wider than most people
expect. Where a figure says "about", the app holds one typical value rather than a range. Treat
all of it as somewhere to begin, then measure — shrinkage and flow especially, because those two
are what throw dimensions off.
Nozzle
185–220 °C (start 200)
Bed
50–65 °C (start 55)
Part fan
80–100% (start 100%)
Wall speed
20–40 mm/s
Max volumetric flow
about 7 mm³/s
Shrinkage
about 0.3%
Softens at
about 60 °C
Enclosure
Not needed
Nozzle size
0.5 mm or larger — 0.6 mm recommended
Nozzle material
Brass is fine for occasional use; hardened steel if you print it often
Drying
about 45 °C for 5 h
Speed
MUCH SLOWER, 20–40 mm/s. Speed means more shear and more heat in the melt zone, which scorches the wood particles and turns them into the blockage everyone blames the filament for.
Bed surface
Smooth or textured PEI at 55 °C. It sticks readily.
Nozzle
A 0.4 mm nozzle WILL clog. Wood particles are large and irregular, and they bridge across the opening. 0.5 mm is the practical minimum, 0.6 mm is the comfortable answer. Clogging is the real problem here, not wear: wood flour is soft, so brass survives occasional printing. If you run wood often, hardened steel saves you replacing a nozzle that has quietly opened up and taken your flow calibration with it.
What bites people
Print COOLER than plain PLA. Wood particles scorch above roughly 220 °C, and burnt wood in the melt zone is what causes the notorious clogs.
Use a 0.5 mm nozzle or larger. Wood fibres bridge across a 0.4 mm opening and block it.
Do not leave it sitting hot in the nozzle. Between-print dwell at temperature chars the particles.
The colour darkens as temperature rises — some people exploit this deliberately for shading, but it also means an uneven tower looks like a defect when it is not.
Sands and stains like wood, which is the whole point of using it.
Safety
Nozzle runs above 185 °C.
Mildly abrasive. Brass survives longer than with carbon fibre, but hardened steel is the safer choice.
Common questions
What temperature should I print Wood-filled PLA at?
Start at 200 °C nozzle and 55 °C bed, within a usable range of 185–220 °C and 50–65 °C. Run a temperature tower on your own spool rather than trusting any table: brand-to-brand variation inside one material is wider than most beginners expect.
Does Wood-filled PLA need an enclosure?
No. Wood-filled PLA prints fine on an open-frame machine.
What nozzle do I need for Wood-filled PLA?
0.5 mm or larger, with 0.6 mm recommended. It is mildly abrasive. Brass survives occasional printing; if you run it often, hardened steel stops the nozzle quietly opening up and taking your flow calibration with it.