supplier range These are starting points drawn from
manufacturer data sheets across the material, not measurements of your spool. Shrinkage and
flow especially: treat them as somewhere to begin, then measure.
Speed
SLOWER than PLA — 25–45 mm/s. PETG needs contact time to fuse to the layer below. Run it at PLA speeds and you get parts that look fine and snap cleanly along the layer lines.
Bed surface
Textured PEI is ideal. On SMOOTH PEI, apply glue stick as a RELEASE agent — PETG chemically bonds to bare smooth PEI and will tear the sheet coating off with the part.
What bites people
Sticks too well, not too little. The failure mode is a destroyed build surface, not a part that comes loose.
Wants a slightly HIGHER first-layer Z-offset than PLA. Squishing PETG like PLA is what causes it to weld itself to the plate.
Stringing is often wet filament. Dry first, tune retraction second.
Do not over-cool. Heavy fan looks cleaner but destroys layer adhesion, which is the entire reason to choose PETG over PLA.
Safety
Nozzle above 230 °C. Bed above 70 °C is hot enough to burn.
Common questions
What temperature should I print PETG at?
Start at 240 °C nozzle and 80 °C bed, within a usable range of 225–255 °C and 70–90 °C. Run a temperature tower on your own spool rather than trusting any table: brand-to-brand variation inside one material is wider than most beginners expect.
Does PETG need an enclosure?
Not strictly, but an enclosure helps PETG by keeping draughts off the print.
What nozzle do I need for PETG?
0.4 mm or larger, with 0.4 mm recommended. A brass nozzle is fine.