Nylon (PA6 / PA12) prints at about 265 °C with a 80 °C bed and 0% part cooling. Usable range 245–285 °C nozzle, 60–100 °C bed. Needs an enclosure.
PolyamidePA
Starting settings
starting points Every number here is drawn from
manufacturer data sheets across the material as a whole. None of it is a measurement of the
spool in your hand, and brand-to-brand variation inside one material is wider than most people
expect. Where a figure says "about", the app holds one typical value rather than a range. Treat
all of it as somewhere to begin, then measure — shrinkage and flow especially, because those two
are what throw dimensions off.
Nozzle
245–285 °C (start 265)
Bed
60–100 °C (start 80)
Part fan
0–20% (start 0%)
Wall speed
25–45 mm/s
Max volumetric flow
about 8 mm³/s
Shrinkage
about 1.5%
Glass transition
about 60 °C — not a softening point: parts stay rigid well above it, which is why this is used for hot and load-bearing work
Enclosure
Required
Nozzle size
0.4 mm or larger — 0.6 mm recommended
Nozzle material
Brass is fine
Drying
about 80 °C for 12 h, and print straight from the dryer
Speed
Slower than PLA, 25–45 mm/s, and slower still on the first layer. Nylon needs time to bond, and a rushed first layer curls off a plate it was never going to hold on to.
Bed surface
Garolite (G10) is the classic answer. PEI with a glue-stick layer also works — nylon bonds aggressively to bare PEI.
Nozzle
0.6 mm gives more consistent results. Filled nylon variants also require hardened steel.
What bites people
The most hygroscopic common filament by a wide margin. Almost every "nylon prints terribly" report is wet filament.
Shrinks around 1.5% — by far the worst of the common materials. Dimensional parts need compensation.
Parts keep absorbing moisture after printing and get tougher and slightly larger over days. That is normal.
Safety
Nozzle above 245 °C. Emissions are less studied than ABS — ventilate anyway.
Glass-filled and carbon-filled nylon variants are abrasive and require a hardened nozzle.
Common questions
What temperature should I print Nylon (PA6 / PA12) at?
Start at 265 °C nozzle and 80 °C bed, within a usable range of 245–285 °C and 60–100 °C. Run a temperature tower on your own spool rather than trusting any table: brand-to-brand variation inside one material is wider than most beginners expect.
Does Nylon (PA6 / PA12) need an enclosure?
Yes. Nylon (PA6 / PA12) warps and splits without one.
What nozzle do I need for Nylon (PA6 / PA12)?
0.4 mm or larger, with 0.6 mm recommended. A brass nozzle is fine.