By Tony Tate · updated 2026-11-27 · First Layer 1.0.2
ASA prints at about 255 °C with a 100 °C bed and 0% part cooling. Usable range 240–270 °C nozzle, 90–115 °C bed. Needs an enclosure.
Acrylonitrile Styrene Acrylate
Starting settings
starting points Every number here is drawn from
manufacturer data sheets across the material as a whole. None of it is a measurement of the
spool in your hand, and brand-to-brand variation inside one material is wider than most people
expect. Where a figure says "about", the app holds one typical value rather than a range. Treat
all of it as somewhere to begin, then measure — shrinkage and flow especially, because those two
are what throw dimensions off.
Nozzle
240–270 °C (start 255)
Bed
90–115 °C (start 100)
Part fan
0–25% (start 0%)
Wall speed
30–50 mm/s
Max volumetric flow
about 10 mm³/s
Shrinkage
about 0.7%
Softens at
about 100 °C
Enclosure
Required
Nozzle size
0.4 mm or larger — 0.4 mm recommended
Nozzle material
Brass is fine
Drying
about 70 °C for 4 h
Speed
Same as ABS, 30–50 mm/s. Chamber temperature governs success here, not feed rate.
Bed surface
Smooth PEI at 100 °C inside an enclosure.
What bites people
Handles like ABS but holds up outdoors — it is the correct choice for anything that lives in sunlight, where PLA and even PETG degrade.
Same warping behaviour as ABS. Enclosure is not optional.
Safety
Same styrene-family emissions as ABS. Ventilate to outside air or filter properly.
Bed above 90 °C causes contact burns immediately.
Common questions
What temperature should I print ASA at?
Start at 255 °C nozzle and 100 °C bed, within a usable range of 240–270 °C and 90–115 °C. Run a temperature tower on your own spool rather than trusting any table: brand-to-brand variation inside one material is wider than most beginners expect.
Does ASA need an enclosure?
Yes. ASA warps and splits without one.
What nozzle do I need for ASA?